Inconel density & Inconel Properties

Inconel Tensile Strength

  Physical Properties Metric English
Alloy 600 Density 8.47 g/cc 0.306 lb/in³
Alloy 625 Density 8.44 g/cc 0.305 lb/in³
Alloy 718 Density 8.19 0.296 lb/in3 (8.192 g/cm3)

Inconel Alloy 625 Density*. 8440 [kg · m-3]
Inconel Alloy 625 Density: 0.303 lb/in3 (8.44 g/cm3)

Inconel Hardness

Inconel Rockwell Hardness, Inconel Strength

Material Grade Hardness HB
Inconel 625 Round Bar
625
≤ 287 HB
Inconel 625 Plate
625
145-240
Inconel Tube
625
Seamless and Welded
-
Inconel Round Bar
600
65-85B
Inconel Plate
600
65-85B
Inconel Pipe
600
88B max
Inconel Wire
600
-

Inconel Melting Point

Alloy 718 Melting Range Solution Treated: 2500-2600°F
Solution Treated and Aged: 1370-1430°C
Alloy 600 Melting Range Metric: 1354 - 1413 °C
English: 2470 - 2580 °F
Alloy 625 Melting Range 2350 - 2460°F (1280 - 1350°C)

Inconel Electrical Conductivity

Material Conductivity Resistivity Notes
(% IACS) (Siemens/m) (Ohm-m)  

Inconel 600

1.70

9.860E+05

1.014E-06

conductivity converted from resistivity

Inconel 600

1.67

1.030E-06

conductivity converted from resistivity

Inconel 601

1.45

1.190E-06

conductivity converted from resistivity

Inconel 617

1.41

1.220E-06

conductivity converted from resistivity

Inconel 625

1.34

1.290E-06

conductivity converted from resistivity

Inconel 690

11.65

1.480E-07

conductivity converted from resistivity

Inconel 718

1.38

1.250E-06

conductivity converted from resistivity

Inconel X750

1.41

1.220E-06

conductivity converted from resistivity

Inconel Heat Treatment

Heat Treatment Alloy 600 Alloy 600 is not an age hardening alloy; cold working is the only available means of hardening. Softening by annealing begins at about 1600°F (871°C), and is reasonably complete after 10 to 15 minutes of heating at 1800°F (982°C). Above this temperature, grain growth may be objectionable, although very brief heating at 1900°F will cause complete softening without undue grain growth. Since the rate of cooling has no effect on the softening, the material may be water quenched or air cooled.
Heat Treatment Alloy 625 Alloy 625 has three basic heat treatments:
(1) High Solution Anneal - 2000/2200°F (1093/1204°C), air quench or faster.
(2) Low Solution Anneal - 1700/1900°F (927/1038°C), air quench or faster.
(3) Stress Relieve - 1650°F (899°C), air quench.
Heat Shield Inconel (2200 deg F continuous).

Inconel Low Temperature

Alloy 718 temperature ranges from cryogenic up to 1400°F
Alloy 625 temperatures ranging from cryogenic to 2000°F

Inconel Temperature Limits

Alloy 600 Heat Capacity

Metric: 0.444 J/g-°C
English: 0.106 BTU/lb-°F

Alloy 625 Heat Capacity Metric: 0.41 J/g-°C
English: 0.098 BTU/lb-°F

Inconel Thermal Conductivity

Thermal Properties and Expansion

Alloy 600 Thermal Conductivity

Metric: 14.9 W/m-K
English: 103 BTU-in/hr-ft²-°F

Alloy 625 Thermal Conductivity Metric: 9.8 W/m-K
English: 68 BTU-in/hr-ft²-°F

Typical Mechanical Properties of Inconel

Inconel Machinability and Inconel Yield Strength

Material Grade Form and Condition Tensile Strength Yield Strength Elongation % Hardness, Rockwell
ksi MPa ksi MPa
Inconel Round Bar 600 Cold drawn Annealed 80-100 550-690 25-50 170-345 55-35 65-85B
Inconel Plate 600 Hot rolled Annealed 80-100 550-725 30-50 205-345 55-35 65-85B
Inconel Plate 600 Cold Rolled Annealed 80-100 550-690 30-45 205-310 55-35 88B max
Inconel Pipe 600 Cold Drawn Annealed 80-100 550-690 25-50 170-345 55-35 88B max
Inconel Wire 600 Cold Drawn Annealed 80-120 550-830 35-75 240-520 45-20 -
Inconel 625 Round Bar 625 Annealed 120 827 60 414 30 ≤ 287 HB
Inconel 625 Plate 625 Annealed 120 827 60 414 30 145-240
Inconel Tube 625
Seamless and Welded
Annealed 120 827 60 414 35 -